December 28, 2021

4. Movable template bending

When the mold is injected, the molten plastic in the cavity produces a huge back pressure, generally 600 ~ 1000 kg/cm2. Mold makers sometimes do not pay attention to this problem, and often change the original design size, or replace the movable template with low-strength steel plate. In the mold with ejector pin, the large span between the two sides of the seat causes the template to bend during injection.

Therefore, the movable formwork must be made of high-quality steel, with sufficient thickness, and low-strength steel plates such as A3 should not be used. When necessary, support columns or support blocks should be set under the movable formwork to reduce the thickness of the formwork and increase the load-bearing capacity.

The above is the How to troubleshoot the failure of the injection mold?-part4 we have listed for you. You can submit the following form to obtain more industry information we provide for you.

You can visit our website or contact us, and we will provide the latest consultation and solutions

Share to:

Send Inquiry

Home> Industry Information> How to troubleshoot the failure of the injection mold?-part4

Send Inquiry

Cheryl

Ms. Cheryl

Email:

Send Inquiry

Tel:+86-576-88807095

Fax:

Mobile Phone:+8613905763982

Email:

Address:Shangnian Industrial Area, Taizhou, Zhejiang

Mobile Site

Home

Product

Phone

About Us

Inquiry

We will contact you immediately

Fill in more information so that we can get in touch with you faster

Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.

Send